Abstract
Nowadays the traditional Sn-Pb brazing alloys have been replaced by alternative solder alloys. This is due to the recognized hazardousness of lead, whose complete market exclusion is predicted as unavoidable in few years. The brazing process is widely used to connect microelectronic devices. The eutectic Sn-Pb presents adequate properties to be applied in brazing and soldering processes, …