Adhesion Evaluation of Dentin Sealing, Micropermeability, and Bond Strength of Current HEMA-free Adhesives to Dentin

Texto completo
Autor(es):
Bacelar-Sa, Renata [1] ; Sauro, Salvatore [2] ; Abuna, Gabriel [1] ; Vitti, Rafael Pino [3] ; Nikaido, Toru [4] ; Tagami, Junji [4] ; Bovi Ambrosano, Glaucia Maria [5] ; Giannini, Marcelo [1]
Número total de Autores: 8
Afiliação do(s) autor(es):
[1] Univ Estadual Campinas, Dept Restorat Dent, Piracicaba Dent Sch, Piracicaba, SP - Brazil
[2] CEU Cardenal Herrera Univ, Fac Hlth Sci, Dent Dept, Prevent & Minimally Invas Dent, Dent Biomat, Valencia - Spain
[3] Univ Taubate, Dept Dent, Taubate, SP - Brazil
[4] Tokyo Med & Dent Univ, Cariol & Operat Dent, Dept Restorat Sci, Grad Sch Med & Dent Sci, Tokyo - Japan
[5] Univ Estadual Campinas, Piracicaba Dent Sch, Dept Social Dent, Piracicaba, SP - Brazil
Número total de Afiliações: 5
Tipo de documento: Artigo Científico
Fonte: Journal of Adhesive Dentistry; v. 19, n. 4, p. 357-364, 2017.
Citações Web of Science: 0
Resumo

Purpose: To evaluate dentin sealing (DS), micropermeability (MP), and dentin bond strength (BS) of HEMA-free adhesives after 24 h and one year of artificial saliva storage. Materials and Methods: Two HEMA-free (G-ae nial Bond and BeautiBond) and All-Bond 3 (the bottle of resin is HEMA-free) adhesives were tested. Adper Single Bond 2, a HEMA-containing adhesive, served as the control. All adhesives were applied according to the manufacturers' instructions and teeth were prepared for DS (n = 5), MP (n = 5), and BS testing (n = 10). DS under a pulpal pressure of 10 psi was performed at 4 time points (when smear layer was present, after EDTA treatment, after adhesive application, and after 1 year). MP was assessed using pulpal pressure of a 20-cm aqueous dye-solution column and confocal laser scanning microscopy. DS, MP, and BS were performed after 24 h or one-year storage. BS and DS data were statistically analyzed using two-way ANOVA, the Tukey-Kramer test (for BS) and Tukey's post-hoc test (for DS) (alpha = 0.05). A qualitative MP assessment was performed by comparing the accumulation of yellow dye within the resin-dentin interface. Results: Adper Single Bond 2 and All-Bond 3 completely sealed the dentin at 24 h and one year. G-ae nial Bond showed statistically significant DS reduction of approximately 15% after one year. BeautiBond showed no DS reduction after one year. The resin-dentin interface created using Adper Single Bond 2 and GA showed dye accumulation primarily after one year. The mean BS of All-Bond 3 was statistically significantly higher than that of other adhesives, while G-ae nial Bond and BeautiBond showed statistically significantly lower mean bond strengths than did Adper Single Bond 2 and All-Bond 3. After one-year storage, the mean BS was statistically significantly lower only for G-ae nial Bond. Conclusion: DS, MP, and BS were not influenced by the absence of HEMA in the tested adhesives. (AU)

Processo FAPESP: 12/19023-8 - Avaliação da permeabilidade dentinária e da resistência de união à dentina imediata e a longo prazo de sistemas adesivos que não contém HEMA
Beneficiário:Marcelo Giannini
Modalidade de apoio: Auxílio à Pesquisa - Regular
Processo FAPESP: 11/11415-1 - Estudo da união dentina-sistemas adesivos que não contém HEMA: avaliação do selamento dentinário, da micropermeabildade e da resistência de união à dentina imediata e a longo prazo.
Beneficiário:Renata Bacelar Cantanhede de Sá
Modalidade de apoio: Bolsas no Brasil - Doutorado