Optimization of Anodization Parameters in Ti-30Ta Alloy

Texto completo
Autor(es):
Capellato, Patricia [1] ; Sachs, Daniela [1] ; Vasconcelos, Lucas V. B. [1] ; Melo, Miriam M. [2] ; Silva, Gilbert [2] ; Ranieri, Maria G. A. [3] ; Zavaglia, Cecilia A. de C. [4] ; Nakazato, Roberto Z. [5] ; Alves Claro, Ana P. R. [6]
Número total de Autores: 9
Afiliação do(s) autor(es):
[1] Unifei Fed Univ Itajuba, Inst Phys & Chem, Av BPS 1303, BR-37500903 Itajuba, MG - Brazil
[2] Unifei Fed Univ Itajuba, Inst Mech Engn, Av BPS 1303, BR-37500903 Itajuba, MG - Brazil
[3] Unifei Fed Univ Itajuba, Inst Prod Engn & Management, Dev Technol & Soc Program DTEcS, Av BPS 1303, BR-37500903 Itajuba, MG - Brazil
[4] Univ Estadual Campinas, UNICAMP, Fac Mech Engn, Rua Mendeleyev 200, BR-13083860 Campinas, SP - Brazil
[5] Sao Paulo State Univ, Sch Engn, Dept Chem & Energy, UNESP, Av Ariberto Pereira da Cunha 333, BR-12516410 Guaratingueta, SP - Brazil
[6] Sao Paulo State Univ, Sch Engn, Mat & Technol Dept, UNESP, Av Ariberto Pereira da Cunha 333, BR-12516410 Guaratingueta, SP - Brazil
Número total de Afiliações: 6
Tipo de documento: Artigo Científico
Fonte: METALS; v. 10, n. 8 AUG 2020.
Citações Web of Science: 0
Resumo

The current metallic biomaterial still presents failures associated with the bulk alloy and the interface of material/human body. In previous studies, titanium alloy with tantalum showed the elastic modulus decrease in comparison with that of commercially pure (cp) titanium. In this study, surface modification on Ti-30Ta alloy was investigated. Titanium and tantalum were melted, homogenized, cold-worked by a rotary swaging process and solubilized. The anodization process was performed in electrolyte contained glycerol + NH4F 0.25% at 30 V using seven different durations-4 h, 5 h, 6 h, 7 h, 8 h, 9 h, and 10 h and annealed at 530 degrees C for 1 h. The surface topography was characterized by scanning electron microscopy (SEM), atomic force microscopy (AFM) measurements, X-ray diffraction analysis (XRD), and contact angle. From the results, we conclude the time of anodization process influences the shape and morphology of the anodized layer. The 5 h-anodization process produced a smooth and porous surface. The 4-, 6-, 7-, 8-, 9-, and 10-h conditions showed nanotubes morphology. All surfaces are hydrophilic (<90 degrees). Likewise, all the investigated conditions present anatase phase. So, this surface modification presents potential for biomedical application. However, more work needs to be done to better understand the influence of time on the anodization process. (AU)

Processo FAPESP: 14/14533-3 - Estudo do emprego da eletrofiação de PCL na superfície da liga Ti-30Ta após crescimento de nanotubos de TiO2
Beneficiário:Patricia Capellato
Modalidade de apoio: Bolsas no Brasil - Pós-Doutorado