The anodising behaviour of four high-strength aluminium alloys (AA2024-T3, AA2198-T8, AA2198-T851, and AA7475-T761) in tartaric-sulphuric acid (TSA) under identical constant voltage conditions was investigated. Significant differences were found in current density, anodic film thickness, and anodising efficiency. An inverse relationship was observed between total charge consumption and film thickness. Among the alloys, AA7475-T761 exhibited the greatest film thickness and highest efficiency, whereas AA2024-T3 showed the highest charge consumption and the thinnest film. The Al-Cu-Li alloys exhibited similar anodising behaviour. All anodic films revealed porous, sponge-like morphologies attributed to oxygen evolution. Variations in film thickness are correlated to alloy compositions. (AU) | |
| Processo FAPESP: | 19/18388-1 - Efeito da microestrutura de ligas de Al de alta resistência na formação e comportamento frente à corrosão da camada anodizada |
| Beneficiário: | João Victor de Sousa Araujo |
| Modalidade de apoio: | Bolsas no Brasil - Doutorado |
| Processo FAPESP: | 22/06935-0 - Caracterização da microestrutura da camada anodizada em ligas de Al por meio de técnicas de alta magnificação e resolução espacial |
| Beneficiário: | João Victor de Sousa Araujo |
| Modalidade de apoio: | Bolsas no Exterior - Estágio de Pesquisa - Doutorado |