Busca avançada
Ano de início
Entree
(Referência obtida automaticamente do Web of Science, por meio da informação sobre o financiamento pela FAPESP e o número do processo correspondente, incluída na publicação pelos autores.)

Effect of zirconia decontamination protocols on bond strength and surface wettability

Texto completo
Autor(es):
Noronha, Mayara dos Santos [1] ; Fronza, Bruna Marin [2] ; Andre, Carolina Bosso [3] ; de Castro, Eduardo Fernandes [1] ; Soto-Montero, Jorge [1] ; Price, Richard Bengt [4] ; Giannini, Marcelo [1]
Número total de Autores: 7
Afiliação do(s) autor(es):
[1] Univ Estadual Campinas, Piracicaba Dent Sch, Dept Restorat Dent, Piracicaba, SP - Brazil
[2] Univ Sao Paulo, Sch Dent, Dept Biomat & Oral Biol, Sao Paulo, SP - Brazil
[3] Univ Fed Minas Gerais, Sch Dent, Dept Restorat Dent, Ave Presidente Antonio Carlos, 6627, BR-31270901 Belo Horizonte, MG - Brazil
[4] Dalhousie Univ, Sch Dent, Dept Clin Dent Sci, Halifax, NS - Canada
Número total de Afiliações: 4
Tipo de documento: Artigo Científico
Fonte: Journal of Esthetic and Restorative Dentistry; v. 32, n. 5 JUN 2020.
Citações Web of Science: 0
Resumo

Objective To evaluate the effects of human saliva decontamination protocols on bond strength of resin cement to zirconia (Y-PSZ), wettability, and microbial decontamination. Materials and methods Zirconia plates were sandblasted and divided into (a) not contaminated, (b) contaminated with human saliva and: (c) not cleaned, (d) cleaned with air-water spray, (e) cleaned with 70% ethanol, (f) cleaned with Ivoclean, or (g) cleaned with nonthermal atmospheric plasma (NTAP). The wettability and microbial decontamination of the surfaces were determined after saliva contamination or cleaning. Monobond Plus (Ivoclar Vivadent) was applied after cleaning, followed by Variolink LC (Ivoclar Vivadent). The samples were stored 1 week before shear bond strength (SBS) testing, and data (SBS and wettability) were analyzed by one-way analysis of variance and Tukey test (alpha= .05). Results Saliva contamination reduced SBS to zirconia compared to not contaminated. Both Ivoclean and NTAP produced higher SBS compared to not cleaned and were not significantly different from the not contaminated. Ivoclean produced the highest contact angle, and NTAP the lowest. With the exception of using just water-spray, all cleaning protocols decontaminated the specimens. Conclusions Both Ivoclean and NTAP overcame the effects of saliva contamination, producing an SBS to zirconia comparable to the positive control. Clinical significance Dental ceramics should be cleaned prior to resin cementation to eliminate the effects of human saliva contamination, and Ivoclean and NTAP are considered suitable materials for this purpose. (AU)

Processo FAPESP: 17/50131-5 - Effect of argon plasma and primer application on the bond strength of resin cements to two yttrium-tetragonal zirconia polycrystal ceramics
Beneficiário:Marcelo Giannini
Modalidade de apoio: Auxílio à Pesquisa - Regular