Polyphenol-enriched extract of Arrabidaea chica used as a dentin pretreatment or incorporated into a total-etching adhesive system: Effects on bonding stability and physical characterization

Texto completo
Autor(es):
Mostrar menos -
Mendes, Bruna Novaes [1] ; Bridi, Enrico Coser [1] ; Franca, Fabiana Mantovani Gomes [1] ; Turssi, Cecilia Pedroso [1] ; do Amaral, Flavia Lucisano Botelho [1] ; Basting, Rosanna Tarkany [1] ; Sousa, Ilza Maria de Oliveira [2] ; da Silva, Tania Mara [3] ; Goncalves, Sergio Eduardo de Paiva [3] ; Foglio, Mary Ann [2] ; Basting, Roberta Tarkany [1]
Número total de Autores: 11
Afiliação do(s) autor(es):
[1] Sao Leopoldo Mand Res Inst, Rua Jose Rocha Junqueira 13, BR-13045755 Sao Paulo - Brazil
[2] Univ Estadual Campinas, Fac Pharmaceut Sci, POB 6029, BR-13083859 Campinas, SP - Brazil
[3] UNESP Univ State Sao Paulo, Inst Sci & Technol Sao Jose dos Campos, Ave Engn Francisco Jose Longo 777, BR-12245000 Sao Jose Dos Campos, SP - Brazil
Número total de Afiliações: 3
Tipo de documento: Artigo Científico
Fonte: Materials Science & Engineering C-Materials for Biological Applications; v. 116, NOV 2020.
Citações Web of Science: 0
Resumo

The aim of this paper was to evaluate the physical properties and the long-term bond strength of a 2.5% polyphenol-enriched extract of Arrabidaea chica (AC) incorporated into both the phosphoric acid and the primer of a three-step total-etch adhesive, or into an aqueous solution as a dentin pretreatment. Fifty dentin surfaces received the treatments (n = 10): CON (control) - application of the three-step adhesive system (Adper Scotchbond Multipurpose, 3M ESPE); WAT - distilled water used as a pretreatment after dentin etching and before application of the adhesive system; ACPA -AC incorporated into the phosphoric acid; ACW - dentin pretreatment with AC incorporated into an aqueous solution after etching; ACP - AC incorporated into the primer. Microtensile bond strength tests were performed after 24 h, 6 and 12 months of storage. Slices from the resindentin interface were obtained for scanning electron microscopy analysis of the hybrid layer. Degree of conversion of AC incorporated into the primer was evaluated. The particle size, polydispersity index and zeta potential of all the solutions prepared by incorporating AC (phosphoric acid, primer and distilled water) were measured by dynamic light scattering, which brought about changes after incorporation. Degree of conversion of the primer was not affected after incorporating AC. ACP showed lower microtensile bond strength values than the other groups. Bond strength decreased after 6 months of storage, stabilizing at the 12-month evaluation. Therefore, use of AC incorporated into the primer led to lower bond strength values, since AC modified the physical properties (particle size, polydispersity index and zeta potential) of the primer, but did not change the degree of conversion. Application of AC as a dentin pretreatment did not affect bond strength or the micromorphological characteristics of the hybrid layer. (AU)

Processo FAPESP: 17/08082-7 - Arrabidaea chica incorporado ao ácido fosfórico e ao primer de um sistema adesivo convencional ou como pré-tratamento dentinário em solução aquosa: avaliação das propriedades físicas das soluções e influência nas propriedades físico-mecânicas da dentina
Beneficiário:Roberta Tarkany Basting Höfling
Modalidade de apoio: Auxílio à Pesquisa - Regular
Processo FAPESP: 16/04343-8 - Extrato de Arrabidaea chica aplicado como pré-tratamento dentinário ou quando incorporado a um sistema adesivo convencional: influência na longevidade da resistência de união
Beneficiário:Bruna Novaes Mendes
Modalidade de apoio: Bolsas no Brasil - Iniciação Científica