Stain resistance and surface roughness of CAD/CAM processed hybrid ceramic

Texto completo
Autor(es):
Silva, Ana Leticia Franklin [1] ; Geng-Vivanco, Rocio [1] ; Tonani-Torrieri, Rafaella [1] ; Pires-de-Souza, Fernanda de Carvalho Panzeri [1]
Número total de Autores: 4
Afiliação do(s) autor(es):
[1] Univ Sao Paulo, Dept Dent Mat & Prosthodont, Ribeirao Preto Sch Dent, Ave Cafe S-N, BR-14040904 Ribeirao Preto, SP - Brazil
Número total de Afiliações: 1
Tipo de documento: Artigo Científico
Fonte: COLOR RESEARCH AND APPLICATION; v. 46, n. 4, p. 901-908, AUG 2021.
Citações Web of Science: 0
Resumo

This study evaluated the stain resistance and surface roughness alteration of a CAD/CAM processed hybrid ceramic. Specimens were fabricated: 30 of resin-based composite (RBC; Filtek Z350), 30 of ceramic (IPS emax Press) and 60 of hybrid ceramic (Lava Ultimate). Color, translucency (BYK Gardner), whiteness index for dentistry (WID) and surface roughness (Surftest SJ-201P) measurements were made. Samples were randomly separated into three groups: Coffee staining (3 hours/day), coffee staining + mechanical toothbrushing (3 hours/day-staining + 40 cycles-toothbrushing) and storage in distilled water (control), all for 30 days Afterwards, all specimens were polished: RBC (n = 10) with a composite polishing kit (Enhance Dentsply), ceramic (n = 10) with a ceramic one (Eve Diapol), half of the hybrid ceramic (n = 10) with the composite polishing kit and the other half (n = 10) with the ceramic kit. Then, final readouts were obtained. Data was analyzed by two-way analysis of variance. The hybrid ceramic exhibited intermediate color change after staining (P < .05). The hybrid ceramic presented WID chance similar to ceramic in control group (P > .05). After staining/brushing, the hybrid ceramic polishing with the ceramic kit revealed the greatest translucency change (P < .05). RBC and hybrid ceramic polishing with the resin kit presented similar surface roughness alteration (P > .05), except after staining/brushing (P < .05). Also, ceramic was different from the hybrid ceramic polishing with the ceramic kit (P < .05). The hybrid ceramic showed intermediate staining and roughness compared to the RBC and the ceramic. The ceramic polishing kit was more effective in removing stains from the hybrid ceramic. (AU)