Busca avançada
Ano de início
Entree
(Referência obtida automaticamente do Web of Science, por meio da informação sobre o financiamento pela FAPESP e o número do processo correspondente, incluída na publicação pelos autores.)

Texto completo
Autor(es):
Mostrar menos -
Aveiro, L. R. [1] ; Da Silva, A. G. M. [2] ; Candido, E. G. [2] ; Antonin, V. S. [1, 3] ; Parreira, L. S. [2] ; Papai, R. [1] ; Gaubeur, I [1] ; Silva, Fernando L. [3] ; Lanza, V, M. R. ; Camargo, P. H. C. [2] ; Santos, M. C. [1]
Número total de Autores: 11
Afiliação do(s) autor(es):
[1] Fed Univ ABC, UFABC, Ctr Nat & Human Sci, Lab Electrochem & Nanostruct Mat, BR-09210170 St Andre - Brazil
[2] Univ Sao Paulo, Inst Chem, Av Prof Lineu Prestes 748, BR-05508000 Sao Paulo - Brazil
[3] V, Univ Sao Paulo, Inst Chem Sao Carlos, Av Prof Lineu Prestes 748, BR-13560970 Sao Carlos, SP - Brazil
Número total de Afiliações: 3
Tipo de documento: Artigo Científico
Fonte: Chemosphere; v. 208, p. 131-138, OCT 2018.
Citações Web of Science: 8
Resumo

This work describes the electrochemical degradation of Reactive Black 5 (RB5) by two methods: electrochemical and photo-assisted electrochemical degradation with and without a Fenton reagent. Two anodes were used, Pt and boron-doped diamond (BDD, 2500 ppm), and the cathode was 3% MnO2 nanoflowers (NFMnO2) on a carbon gas diffusion electrode (GDE). An electrochemical cell without a divider with a GDE with 3% w/w NFMnO2/C supported on carbon Vulcan XC72 was used. The decolorization efficiency was monitored by UV-vis spectroscopy, and the degradation was monitored by Total Organic Carbon (TOC) analysis. For dissolution monitoring, aliquots (1 mL) were collected during the degradation. After 6 h of H2O2 electrogeneration, the manganese concentration in the RB5 solution was only 23.1 +/- 1.214 mu g L-1. It was estimated that approximately 60 mu g L-1 (<0.2%) of manganese migrated from the GDE to the solution after 12 h of electrolysis, which indicated the good stability of the GDE. The photoelectro-Fenton-BDD (PEF-BDD) processes showed both the best color removal percentage (similar to 93%) and 91% of mineralization. The 3% NFMnO2/C GDE is promising for RB5 degradation. (C) 2018 Elsevier Ltd. All rights reserved. (AU)

Processo FAPESP: 16/00819-8 - Síntese Controlada de Nanomateriais baseados em Pd e Pt: Otimizando Atividade e Estabilidade Eletrocatalítica
Beneficiário:Luanna Silveira Parreira
Modalidade de apoio: Bolsas no Brasil - Pós-Doutorado
Processo FAPESP: 15/10314-8 - Nanoestruturas para a Degradação de Fenol, Ciprofloxacino e 17 alfa etinilestradiol
Beneficiário:Mauro Coelho dos Santos
Modalidade de apoio: Auxílio à Pesquisa - Regular
Processo FAPESP: 17/21846-6 - Nanoestruturas para a remediação ambiental e produção de energia a partir de fontes renováveis
Beneficiário:Mauro Coelho dos Santos
Modalidade de apoio: Auxílio à Pesquisa - Programa BIOEN - Regular