Busca avançada
Ano de início
Entree
(Referência obtida automaticamente do Web of Science, por meio da informação sobre o financiamento pela FAPESP e o número do processo correspondente, incluída na publicação pelos autores.)

Bond Strength of Two-Step Etch-and-Rinse Adhesive Systems to the Dentin of Primary and Permanent Teeth

Texto completo
Autor(es):
Ricci, Herica Adad ; Sanabe, Mariane Emi ; de Souza Costa, Carlos Alberto [1] ; Hebling, Josimeri [2]
Número total de Autores: 4
Afiliação do(s) autor(es):
[1] Univ Estadual Paulista, UNESP, Dept Physiol & Pathol, Araraquara Sch Dent, BR-14801903 Araraquara, SP - Brazil
[2] Univ Estadual Paulista, UNESP, Fac Odontol Araraquara, Dept Orthodont & Pediat Dent, Araraquare Sch Dent, BR-14801903 Araraquara, SP - Brazil
Número total de Afiliações: 2
Tipo de documento: Artigo Científico
Fonte: Journal of Clinical Pediatric Dentistry; v. 35, n. 2, p. 163-168, WIN 2010.
Citações Web of Science: 9
Resumo

Objective: The purpose of this study was to compare the immediate microtensile bond strength (mu TBS) of two-step etch-and-rinse adhesive systems to the dentin of primary and permanent teeth. Study Design: Non-carious human teeth (12 primary molars and 12 premolars) were assigned to 3 groups according to the adhesive system. The adhesive systems were applied to flat superficial coronal dentin surfaces etched with phosphoric acid and composite resin blocks were built up. The teeth were sectioned to produce beam-shaped specimens with 0.81 mm(2) cross-sectional area subjected to mu TBS testing. mu TBS data were analyzed statistically by ANOVA and Tukey's test (a= 0.05). Results: The adhesive systems produced statistically similar mean mu TBS to each other (p> 0.05) and no significant differences (p> 0.05) were found when the same material was applied to primary or permanent tooth dentin. The mean mu TBS values (MPa) obtained were: Prime \& Bond NT: 41.7 +/- 14.4 (permanent) and 40.8 +/- 13.4 (primary); Single Bond: 42.9 +/- 8.6 (permanent) and 41.4 +/- 11.9 (primary); Excite DSC: 46.3 +/- 11.3 (permanent teeth) and 43.4 +/- 12.0 (primary). Conclusion: There was no difference in the immediate mu TBS of two-step etch-and-rinse adhesive systems when applied to the dentin of primary and permanent teeth. (AU)

Processo FAPESP: 06/01781-2 - Efeito da clorexidina na resistencia de uniao de sistemas adesivos a dentina in vitro (decidua e permanente) e na longevidade da interface adesiva in vivo.