Quantitative fractography of fatigue crack propagation surfaces for aircraft alloys

Grant number: 10/02721-9
Support type:Scholarships in Brazil - Master
Effective date (Start): September 01, 2010
Effective date (End): March 31, 2011
Field of knowledge:Engineering - Aerospace Engineering
Principal researcher:Luis Rogerio de Oliveira Hein
Grantee:Thaís Peres Zanetine Marques
Home Institution: Faculdade de Engenharia (FEG). Universidade Estadual Paulista (UNESP). Campus de Guaratinguetá. Guaratinguetá , SP, Brazil
News published in Agência FAPESP Newsletter about the scholarship:
Articles published in other media outlets (0 total):
More itemsLess items
VEICULO: TITULO (DATA)
VEICULO: TITULO (DATA)

Academic Publications
(References retrieved automatically from State of São Paulo Research Institutions)
. Fractografia quantitativa de superfícies obtidas em ensaios de propagação de trincas por fadiga em aço inoxidável 15 –5PH. 2012. Master's Dissertation - Universidade Estadual Paulista (Unesp). Faculdade de Engenharia. Guaratinguetá Guaratinguetá.

Please report errors in scientific publications list by writing to: cdi@fapesp.br.