Hybrid metal oxide cluster@MOF catalysts: design, synthesis by atomic layer deposi...
New multifunctional metal-organic framework catalysts for mild oxidation of methan...
Catalysis-nanostructure-properties relations: establishing basis for the design of...
Sub-monolayer control of the growth of ZrO2 films over ordered mesoporous silica s...
Preparation of nanocatalysts with controlled morphology for applications in hydrog...
Relation between size, composition and structures of Co-Ni nanoparticles and its i...
Nanohybrids photocatalyst AuPd/g-C3N4 nanosheets to promote CH4 oxidation into met...