Advanced search
Start date
Betweenand
(Reference retrieved automatically from SciELO through information on FAPESP grant and its corresponding number as mentioned in the publication by the authors.)

Cross laminated timber bonding quality for different Brazilian species and pressing levels

Full text
Author(s):
João Vítor Felippe Silva [1] ; Karina Aparecida de Aparecida de Oliveira [2] ; Carolina Aparecida Barros Oliveira [3] ; Maria Fernanda Felippe Silva [4] ; Julio Cesar Molina [5]
Total Authors: 5
Affiliation:
[1] Universidade Estadual Paulista. Departamento de Engenharia Mecânica - Brasil
[2] Universidade Estadual Paulista. Departamento de Engenharia Mecânica - Brasil
[3] Universidade Estadual Paulista. Departamento de Engenharia Mecânica - Brasil
[4] Universidade Estadual Paulista. Departamento de Engenharia Industrial Madeireira - Brasil
[5] Universidade de São Paulo. Departamento de Engenharia de Estruturas - Brasil
Total Affiliations: 5
Document type: Journal article
Source: Maderas : Ciencia y tecnología; v. 26, 2023-09-14.
Abstract

Abstract: The proper choice of raw materials and manufacturing parameters for Cross Laminated Timber is essential to promote the proper bonding of the lamellas, aiming at their application in construction. However, few Brazilian species are currently used in the production of Cross Laminated Timber. The aim of this work was to characterize the bonding quality of four Brazilian reforestation species (Pinus elliottii (pino ellioti), Eucalyptus grandis (eucalipto), Toona ciliata (toona) and Acrocarpus fraxinifolius (lazcar)) in the manufacture of Cross Laminated Timber with two-component polyurethane adhesive and five different pressure levels (from 0,1 MPa to 1,3 MPa). Bonding quality was evaluated through delamination and glue line shear tests based on the European standard. Delamination was affected by the wood species, and the best adhesion occurred for the Cross Laminated Timber manufactured with Pinus elliottii (pino ellioti) and Acrocarpus fraxinifolius (lazcar) at the bonding pressure of 0,7 MPa. Cross Laminated Timber bonding pressure did not affect the percentage of wood in the shear test fractured surface, whereas higher density Cross Laminated Timber showed higher percentages. (AU)

FAPESP's process: 20/00555-6 - NUMERICAL AND EXPERIMENTAL STUDY OF THE MAIN PARAMETERS OF RESISTANCE AND STIFFNESS OF CROSS LAMINATED TIMBER ELEMENTS