Advanced search
Start date
Betweenand
(Reference retrieved automatically from Web of Science through information on FAPESP grant and its corresponding number as mentioned in the publication by the authors.)

Effect of the application of a casein phosphopeptide-amorphous calcium phosphate (CPP-ACP) paste and adhesive systems on bond durability of a fissure sealant

Full text
Author(s):
Dutra Borges, Boniek Castillo [1] ; Catelan, Anderson [2] ; Sasaki, Robson Tetsuo [2] ; Bovi Ambrosano, Glaucia Maria [2] ; Reis, Andre Figueiredo [3] ; Baggio Aguiar, Flavio Henrique [2]
Total Authors: 6
Affiliation:
[1] Laureate Int Univ, Potiguar Univ, Sch Dent, Dept Dent, BR-59056000 Natal, RN - Brazil
[2] State Univ Campinas UNICAMP, Piracicaba Dent Sch, Dept Restorat Dent, Piracicaba - Brazil
[3] Univ Guarulhos, Dept Operat Dent, Guarulhos, SP - Brazil
Total Affiliations: 3
Document type: Journal article
Source: ODONTOLOGY; v. 101, n. 1, p. 52-59, JAN 2013.
Web of Science Citations: 4
Abstract

This study aimed to evaluate the effect of the previous application of a casein phosphopeptide-amorphous calcium phosphate paste (MI Paste, MI) and adhesive systems on the bond durability of a fissure sealant. Ninety-eight enamel blocks were obtained from proximal surfaces of erupted third molars. Specimens were divided into 14 groups (n = 7) according to the previous application of MI (with and without) and the adhesive systems used (no adhesive system; hydrophobic resin of a three-step etch-and-rinse adhesive system; etch-and-rinse single-bottle adhesive system; all-in-one adhesive system; two-step self-etching adhesive system; additional phosphoric acid conditioning and all-in-one adhesive system; additional phosphoric acid conditioning and two-step self-etching adhesive system). A fissure sealant (Fluroshield) was applied and photoactivated for 20 s. Beams ( 0.7 mm(2)) were prepared for the microtensile bond strength test, which was executed after 24 h or 6 months of water storage. Fractured specimens were analyzed by scanning electronic microscopy. Data were analyzed by two-way ANOVA with repeated measures/Tukey's test (P < 0.05). Groups that received MI application and adhesive systems presented higher means than those groups where MI was not applied. Higher frequency of cohesive failures was observed for groups with MI. Applying a CPP-ACP containing paste on enamel before adhesive systems was an effective method to increase bond durability of the sealant tested. (AU)