Advanced search
Start date
Betweenand
(Reference retrieved automatically from Web of Science through information on FAPESP grant and its corresponding number as mentioned in the publication by the authors.)

Effect of home-bleaching gels modified by calcium and/or fluoride and the application of nano-hydroxyapatite paste on in vitro enamel erosion susceptibility

Full text
Author(s):
Thives Freitas Santos, Luciana Floriani [1] ; Gomes Torres, Carlos Rocha [1] ; Ferraz Caneppele, Taciana Marco [1] ; Magalhaes, Carolina [2] ; Borges, Alessandra Buhler [1]
Total Authors: 5
Affiliation:
[1] Univ Estadual Paulista, UNESP, Inst Sci & Technol, Dept Restorat Dent, BR-12245000 Sao Jose Dos Campos, SP - Brazil
[2] Univ Sao Paulo, Bauru Sch Dent, Dept Biol Sci, Bauru, SP - Brazil
Total Affiliations: 2
Document type: Journal article
Source: ACTA ODONTOLOGICA SCANDINAVICA; v. 74, n. 2, p. 121-126, FEB 17 2016.
Web of Science Citations: 8
Abstract

Objective. This in vitro study compared the effect of bleaching agents modified by the addition of calcium and/or fluoride and the application of a nano-hydroxyapatite paste after bleaching, on the susceptibility of enamel to erosion. Materials and methods. Bovine enamel cylindrical samples (3 mm diameter) were assigned to six groups (n = 20 specimens/group) according to the bleaching agent: no bleaching (C-control), 7.5% hydrogen peroxide gel (HP), HP with 0.5% calcium gluconate (HP+Ca), HP with 0.2% sodium fluoride (HP+F), HP with calcium and fluoride (HP+Ca+F) and HP followed by the application of a nano-hydroxyapatite agent (HP+NanoP). The gels were applied on the enamel surface (1 h) followed by cyclic erosive challenges (Sprite Zero (R)-2 min), for 14 days. The paste was applied after bleaching for 5 min (HP+NanoP). The enamel surface alteration was measured by contact profilometry (mu m) (after 7 and 14 days). Results. C-control (mean +/- SD: 2.29 +/- 0.37 at 7 days/4.86 +/- 0.72 at 14 days) showed significantly lower loss compared to the experimental groups. HP+Ca (3.34 +/- 0.37/6.75 +/- 1.09) and HP+F (4.49 +/- 0.92/7.61 +/- 0.90) presented significantly lower enamel loss than HP (4.18 +/- 0.50/10.30 +/- 1.58) only for 14 days and HP+Ca+F (4.92 +/- 1.03/8.12 +/- 1.52) showed values similar to the HP+F group. The HP+NanoP (5.51 +/- 1.04/9.61 +/- 1.21) resulted in enamel loss similar to the HP after 14 days. Conclusions. It was found that 7.5% hydrogen peroxide increased the susceptibility of enamel to erosion. The addition of calcium or fluoride to the bleaching gel reduced the erosion effect, while the nano-hydroxyapatite agent did not provide any protective effect. (AU)